The samples were fired in an electric kiln over a 2 hour period to 1100° F and held at that temperature for 5 minutes.

Samples are fired "face up"

BEFORE: Unfired samples

AFTER: Fired samples (before removing clay residue). Note the color change of both the clay and the glass compared to the unfired samples above.